Recent Posts
Recent Comments
Adrian on A summary of limewashing a… byrnesurfaces on A summary of limewashing a… Adrian on A summary of limewashing a… byrnesurfaces on A summary of limewashing a… Adrian on A summary of limewashing a… Archives
- February 2023
- November 2022
- January 2022
- November 2021
- November 2020
- July 2018
- October 2017
- April 2017
- March 2017
- January 2017
- December 2016
- August 2016
- March 2016
- January 2016
- November 2015
- May 2015
- April 2015
- March 2014
- November 2013
- October 2013
- September 2013
- September 2012
- July 2012
- May 2012
- January 2012
- November 2011
- September 2011
- January 2011
Categories
Meta
Monthly Archives: October 2013
Nothing need be wasted when using lime
Having finished the harling there was a bit of course stuff left over and the tools needed washing. so both the remaining render and the tool washing water was put in a barrel and, with the addition of more lime, … Continue reading
Posted in limewash, Roughcast render, technical stuff
Leave a comment
Short measures
I am fed up with opening tubs of lime putty and finding that there is not the 15 litres I was expecting, I assume I am being charged for 15 litres so why am I not getting them all? its … Continue reading
Posted in Lime Plaster, technical stuff
Leave a comment